Skip to content
KORNDEX – Home

Sanding problem

Plastic smears and fuzzes instead of sanding

Also: Bumper smearing · Plastic going soft · Fuzz instead of dust

Why does plastic smear when sanding? Speed and pressure soften the surface because plastic conducts heat poorly. Small orbit, low speed, light pressure – and clean release agent off new parts first.

How to spot it

Instead of sanding dust you get fuzz and shiny smeared patches, and the disc clogs within seconds.

Where it comes from

  • Plastic conducts heat poorly: high speed and heavy pressure soften the surface.
  • The mould release agent was not wiped off and got rubbed in by the abrasive.
  • Started too coarse – anything coarser than P180 is rarely needed on plastic.

What helps now

  • Small orbit, low speed, light pressure – better to change the disc once more often.
  • Wipe new parts with plastic cleaner before the first sanding.
  • Smooth scratches with P180, refine with P240 and P320, matt down with P400 before painting; edges and swage lines with non-woven abrasive.

Grits to put it right

Read the full sequence:Plastic

In depth in the guides:What grit sandpaper for plastic? Preparing bumpers What grit before painting?

More sanding defects