Sanding problem

The new paint won’t stick or beads off

Also: Paint peeling · Paint beading · Craters in the paint · Poor adhesion

Why won’t the new paint stick? Usually shiny spots were left or wax, silicone and release agent were sanded into the scratches. Clean first, then matt down evenly, then degrease.

How to spot it

The fresh coat pulls together, beads off in places or can later be lifted with a fingernail.

Where it comes from

  • Shiny spots were left – anything still shiny has not been keyed and gives the paint nothing to hold on to.
  • Polish, wax, silicone or release agent was spread into the scratches while sanding instead of being removed first.
  • The surface was not degreased after sanding or was touched with bare hands.

What helps now

  • Matt down evenly until no shiny spot remains: flat areas with P400 to P600, edges and swage lines with non-woven abrasive.
  • Clean first, then sand – wipe down old furniture and new plastic parts beforehand.
  • Vacuum the dust, degrease with silicone remover, wipe with a tack cloth and do not touch the surface afterwards.

Grits to put it right

Read the full sequence:Primer coat Plastic Wood

In depth in the guides:What grit before painting? Keying and repainting painted furniture What grit sandpaper for plastic? Preparing bumpers